EXPERIMENTAL STUDIES OF BOTTOM ASH AND FIBER OF HIGH STRENGTH MORTAR

Author(s)

K.Jagadish Prasad, R.Suresh

Abstract

The developments of high-strength mortar (HSM) with supplementary cementitious materials(SCM) are in high demand in order to not only enhancing the mechanical properties but also to life span and minimize the maintenance cost of the RC structures. In this experimental investigation, two high strength mortar (HSM) mixes (CM 1:3 and CM 1:2) with w/b ratios of 0.5 and 0.45, respectively as reference mixes with BA replacement (0 – 40%) were selected. Quantity of water for mixes based on flow table test for mortar was assessed. Various mixes incorporating SF varying from 0 – 20 % and GO as additive varying from 0 – 0.2 %, were proportioned. For HSFRM mix (CM 1:3), polypropylene (PP) fibers (Vf = 0- 1%) with SF = 20% were used. The impact energy absorbed by the fibre reinforced mortar slabs were compared with the non-fibrous mortar slabs. It was found that the impact energy at ultimate failure, absorbed by the PP – FRM with Vf = 1% is 80 % more than that of HSM with SF = 20 %, and about 145 % that of HSM with SF = 20 % and GO = 0.15%, which appear to possess relatively a high impact resistance.

Keywords

High-strength mortar; Bottom Ash; Graphene Oxide; Fiber.

Conclusion

Based on the experimental1 investigation carried1 out on the bottom ash1 based high-strength mortar (BA-HSM) 1 with SF and GO and on FRHSM containing PP fibers, the following conclusions are drawn. 1.The rheological1 characteristics of fresh 1cement mortar are decreased with the increase of1 bottom ash (BA) replacement in mortar1 matrix. 2.Beyond 20 % BA replacement, porosity of BA in mortar increases which weakens the transition zone in the mortar. 3.The improvement1 in compressive resistance of 3.5 % for high-strength mortar was obtained at 20 % bottom ash replacement compared1 to control mortar mix which is due1 to fineness of bottom ash filling effect and presence of small quantity of calcium oxide, beyond which there 1is no improvement in strength. 4.1Bottom ash has a high potential to improve the performance of mortar matrix due to its lesser fineness1 and particle size closer1 to that of sand, 1and can be used at 20 % 1replacement of sand for making1 good mortar. 5.Bottom ash replacement of1 fine aggregate in 1cement mortar has 1marginally increased the 1compressive and flexural 1strengths up to 20% BA replacement1 level. 6.Compressive strength of bottom ash based high strength mortars (CM 1:3 and CM 1:2) containing SF = 20%, was improved about 10 % and 14%, respectively, compared to control mortar mix.

References

1. Aggarwal, P., Aggarwal, Y. and Gupta, S.M., 2007, “Effect of Bottom ash as replacement of fine aggregates in concrete”, Asian Journal of Civil Engineering Building and Housing, Vol.8, No.1, pp. 213- 217.
2. Ahmad, O.A, 2017. “Production of high performance silica fume concrete”, American Journal of Applied Sciences, Vol.14, No.11, pp.1031-1038.
3. Ahmed Hadj-sadok., Said Kenai., Luc Courard. and Anne Darimont., 2011, “Microstructure and durability of mortars modified with medium active blast furnace slag”, Construction and Building Materials, Vol.25, No.8, pp. 1018–1025
4. Ali Huddin Ibrahim., Mohammad Ismail., Fauzi Alattas. and Salah Abdulhameed Abdulrahman, 2015, “Effects of coal bottom ash on the compressive strength of Portland cement mortar”, Journal of Building Materials, No.39, No.5, pp.750-820.
5. Ali, M.T. and Chang W.F, 1993, “Strength Properties of Cement Stabilized Municipal solid waste incinerated ash masonry”, Bricksd, ACI Materials Journal, Vol. 91, No.3, pp.256-263.
6. Aly, T., Sanjayan, J. G., Collins F, 2008, “Effect of polypropylene fibres on shrinkage and cracking of concretes Materials and Structures”, Journal of Building Materials, Vol. 08, No.2, pp.286-310.
7. American Society for Testing and Materials, 1990, “ASTM C642, Standard Test Method for Specific Gravity, Water Absorption and Unit Weight of Hardened Concrete”, ASTM Stand. Concrete Aggregate, Vol.4, pp. 318–319.
8. American Society for Testing and Materials, 2004, “ASTM C39-04, Standard Test Method for Compressive Strength of Fiber Reinforced Concrete”, Annual Book of ASTM Standards, ASTM International, USA.
9. American Society for Testing and Materials, 2001, “ASTM C494-01, Standard Specification for Chemical Admixtures for Concrete “, Annual Book of ASTM Standards, ASTM International, USA.
10. American Society for Testing and Materials, 2024, “ASTM C78-04, Standard Test Method for Flexural Strength of Concrete”, Annual Book of ASTM Standards, ASTM International, USA.
11. American Society for Testing and Materials, 2001 “ASTM C494/C494M, is the Standard Specification for Chemical Admixtures for Concrete", Annual Book of ASTM Standards, ASTM International, USA.
12. American Society for Testing and Materials, 2021, “ASTM A820-01, Standard Specification for Steel Reinforced Plastic (SRP) for Use in Underground Applications", Annual Book of ASTM Standards, ASTM International, USA.
13. American Society for Testing and Materials, 2001, “ASTM D3260-01, Standard Guide for the Selection of Methods for the Evaluation of the Effectiveness of the Corrosion Inhibitors in Oil and Gas Production", Annual Book of ASTM Standards, ASTM International, USA.

📋 How to Cite This Paper

K.Jagadish Prasad, R.Suresh (2026). EXPERIMENTAL STUDIES OF BOTTOM ASH AND FIBER OF HIGH STRENGTH MORTAR. International Journal of Engineering and Techniques, 12(6), 459–466. ISSN: 2395-1303. DOI: https://doi.org/10.5281/zenodo.24397876
© 2026 International Journal of Engineering and Techniques (IJET). All rights reserved. · ijetjournal.org

Submit Your Paper